Re: [MW:24619] Lethal service requirement

Dear Sachin,
Check your project specification & process data sheet requirements.

Technically you can perform perform PWHT.

Regards,
Vijay Patre

On Apr 2, 2016 1:01 PM, "sachin sankhe" <sachin.sankhe@rediffmail.com> wrote:
Dear Friends,

Need your opinion on below

Equipment
Columns

Design Code

ASME SEC VIII Div.1

Process 

High Wet H2S service(NACE)
Wet Amine service
Very Toxic
Lethal(ASME SEC VIII, UW-2)

Metallurgy/Thk
Base Metal MOC=SA516 Gr.70
Thk=8mm
Clad MOC=SS316L
Clad thk=3mm

Problem
Is PWHT mandatory for clad vessel for above process condition?
For lethal service is PWHT not mandatory for clad vessel as per Table UCS56.1 Note (e)

Regards
Sachin Sankhe






Get your own FREE website, FREE domain & FREE mobile app with Company email.  
Know More >

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/20160401172500.21291.qmail%40f5mail-224-128.rediffmail.com.
For more options, visit https://groups.google.com/d/optout.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPi2c28zg9DbN%2Bv1Xfmp38ox5i_9-U1Mm%2BZgpqgnFe0gj1pGDg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35354] Cast-iron welding

1. Preheat joint area(other area, cover with mineral wool). 2. ENiCi or ENiFe-CI. 3. stringer bead. 4. peening is to be done on weldmetal im...