Friday, April 1, 2016

Re: [MW:24612] RE: 24605] 3/4" Tube weld RT

Dear sir,
   Please re conduct RT to verify weld profile of initial RT films 

Sent from my iPhone

On Apr 1, 2016, at 09:10, madhusoodhanan Nair <nairdan2@gmail.com> wrote:

Dear sir

  please and the radiography film photo

From: pkkanishk2006@gmail.com
Sent: ‎01-‎04-‎2016 11:33 AM
To: Materials & Welding
Subject: [MW:24605] 3/4" Tube weld RT

Dear Experts ,

I have a situation where external cavity is visible and significant physically on a 3/4" tube weld joint ( welding process - Orbital) , but when we tried to verify through RT DWSI technique its no density variation observed so not able to conclude. Now the vendor is claiming it acceptable , please suggest a way forward and any technique to verify.


Regards
Pratish

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/22d82861-95d1-4217-9b2b-6993b901c46b%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/56fe10e4.890c620a.52f4c.ffff9492%40mx.google.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35354] Cast-iron welding

1. Preheat joint area(other area, cover with mineral wool). 2. ENiCi or ENiFe-CI. 3. stringer bead. 4. peening is to be done on weldmetal im...