generally for GTAW-- 1.5 X Nozzle ID
THANKS & BEST REGARDS,
KG.PANDITHAN, IWE, AWS-CWI, CSWIP 3.1,
CONSULTANT-WELDING & QUALITY
On Fri, Apr 1, 2016 at 10:55 AM, Kannayeram Gnanapandithan <kgpandithan@gmail.com> wrote:
Sec IX, has nowhere said about weaving width for any welding process, but in Section 1 and Section 8, it has given for welding by SMAW, the weaving width may be 4Xcore dia.THANKS & BEST REGARDS,KG.PANDITHAN, IWE, AWS-CWI, CSWIP 3.1,CONSULTANT-WELDING & QUALITYOn Fri, Apr 1, 2016 at 9:47 AM, <pkkanishk2006@gmail.com> wrote:As per sec IX 2.5 times of the electrode dia can be allowed for weaving . In case of GTAW you can consider the tungsten dia in place of electrode dia.--
On Thursday, March 31, 2016 at 5:00:12 PM UTC+5:30, simon lawrence wrote:Pls confirm that Weld weaving width , weld weave maximum how much we can accepted in GTAW process ?
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/ce31dd8b-feec-4270-8bd7-1e585e4deb74%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eN0VcuHj3Y6rVFkOUv4dkWZVxre7DyknE7nzd%2BnioW0Zg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.
Comments