I have to comment, since I do not agree that 'the yield point is observed in all carbon steel material' [but it may depend on what you consider to be a carbon steel]. That statement is probably true for as-rolled and normalised carbon steels but, notably, the TMCP [thermo-mechanical controlled processed] steels which are carbon-manganese micro-alloyed steels and widely used for structures and pipelines do not generally show a distinctive yield point.
Alan Denney
AKD Materials Consulting Ltd
-----Original Message-----
From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Pravin Nimbalkar
Sent: 16 November 2015 07:14
To: Materials & Welding <materials-welding@googlegroups.com>
Subject: Re: [MW:23883] Tensile testing
Definitely
construct a straight line parallel to the initial linear portion of the stress-strain curve, but offset from it by e = 0.002 (0.2%.) The yield strength is taken as the stress level at which this straight line intersects the stress–strain curve.
Generally the yield point is observed in all carbon steel material.
The reason behind yield point is Cottrell atmosphere. Its related to how dislocation pinned in mild steel metals by carbon and nitrogen interstitials. These atoms distort the lattice shortly and there will be associated residual stress field surrounding the interstitials. This stress field relaxed by interestitail atoms diffusing towords dislocation. Once the dislocation has become pinned a small extra force is required to unpinn and the dislocation prior the yielding and produce upper yield point in stress-strain strain diagram. After unpinning dislocation are free to move in Crystal which results means lower yield point and material will deform in more plastic manner.
--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/ca4a0665-8653-4b56-8c30-72e4b23d9a9d%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.
This email has been scanned by BullGuard antivirus protection.
For more info visit www.bullguard.com
--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/000201d12057%249fa02050%24dee060f0%24%40denney1.freeserve.co.uk.
For more options, visit https://groups.google.com/d/optout.
Subscribe to:
Post Comments (Atom)
Re: [MW:35686] HDPE WPS
Refer ASME SEC IX There is separate chapter for Plastic welding . Based on that you have to prepare Sent from my iPhone On 21 Jun 2025, at...
-
Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? ...
-
Definition of buttering from ASME Section IX, QW/QB-492 Definitions: Buttering: the addition of material, by welding, on one or bot...
-
Section I. PRINT READING 3-1. GENERAL a. Drawings . Drawing or sketching is a universal language used to convey all necessary information to...
No comments:
Post a Comment