Re: [MW:23870] Revise was according to EN15614-1

Yes you can without a new PQR provided other parameters are within approval range

Sent from my BlackBerry 10 smartphone.
  Original Message  
From: JERRY TUAN
Sent: Κυριακή, 8 Νοεμβρίου 2015 - 06:13
To: Materials & Welding
Reply To: materials-welding@googlegroups.com
Subject: [MW:23864] Revise was according to EN15614-1

If my pqr . I used butt joint double V, wire diameter 4.8 mm ,process SAW . Now I want to revise wps to used wire diameter 4.0 mm , is this ok
Thanks for help
Tuan.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/78a855f3-c4ca-4428-a39f-eaf687e97905%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.
This message contains confidential information. To know more, please click on the following link: http://disclaimer.bureauveritas.com

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...