Re: [MW:23864] WQT minimum requirement while using 2'' test coupen

No need one test coupon is enough .......
2" is 60.3  multiply by 3.1425 is 189.49mm

On 7 Nov 2015 06:45, "MANIK" <manik.tr2000@gmail.com> wrote:
Dear all

What is the requirements while using 2'' test coupon for WQT?
As i need to prepare 2 numbers of 2" test coupon for one welder.
I assume, it will be minimum circumferential length to be welded, if so how much?
Where shall i find the note in sec IX?

Manik
Piping Supervisor. 

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/202ec153-896e-4bb3-a56c-f998e04eb6f3%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAFFqCZGi68qzVXwOhKZU068qziRqRr92jBNnYT5%2Btn5GLUm5GQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...