Re: [MW:23851] Re: ASTM A36 plates for pressure vessels

Dear syed .

I  hope you are from gerab ,Dubai ,

As per the A 36 plate standard , This plate can not use  in Pipe construction or in the Fitting construction .

because it is structural steel material grade.

where our application of ASTM A 234 WPB fitting is in process piping .

Both are Different ,

We faced same Problem in one of our reputed customer , but finally on the basis of the Chemical composition and mechanical test perform on laboratory and satisfied customer and End users .

Submit one stated letter from the manufacturer to Client about the suitability of  raw material .

Thank you very much 

Best of regards

Ritesh Rajput 



On Tue, Nov 3, 2015 at 8:33 PM, JIGNESH RANA <2010jigs@gmail.com> wrote:
dear Syed, 

strictly,code, there is no limitation on raw material for the products to be certified as per A 234, except it shall meets with chemical requirements of particular grade. 
If specific requirements based on service (like NACE), then restricted chemistry applies. 

regards, 

jignesh rana 

On Tue, Nov 3, 2015 at 11:50 AM, Raghuram Bathula <raghurambathula@gmail.com> wrote:
In addition Code Case 2811 provides guidelines for use of  SA/EN 10025-2 Steel Grades S235J2, S275J2, and S355J2   in fabrication of pressure vessels

https://www.linkedin.com/grp/post/122787-6061068041251278851?trk=groups-post-b-title

On 3 November 2015 at 10:12, Abhay Pethe <agpethe@gmail.com> wrote:
SA-36 is permitted for use in construction of pressure vessels according to UCS-6 of the ASME BPVC. Practically nobody uses the same remains the fact.

No comments regarding the equivalency or use of A36 in place of A234.


Best Regards,
Abhay Pethe

On 30 October 2015 at 06:54, Plate Steel <eric@ysteelplate.com> wrote:
Dear Syed,

Firstly A36 is just one common carbon structural steel,this steel plate can make common tanks,but not pressure vessels.Because,As a professional steel supplier,we knew when rolling A36,no need to do Ultrasonic test,but for pressure vessel used steel,they have to be done Ultrasonic test.

Second,your said A234 is one pressure vessel steel,actually another pressure vessel steel ASTM A285GrC is similar to A234.

It would be dangerous if using A36 to replace of A234,Freind.

Eric 

在 2011年1月24日星期一 UTC+8下午9:36:28,Moin - QC写道:

Dear members,

Can a plate to ASTM A36 can be used to manufacture TEEs to A234 WPB, is there any restriction in BPV or B31.3 on the use of A36 plate for manufacturing A234 Tees.

One of client says A36 is for general purpose and cannot be used for making a pressure containing component to be used in oil and gas production . Is it correct, if yes why? And if not can you please provide me a technical justification, I could not find anything B31.3.

Thanks & Regards
Syed Moin                               


--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADxVubm111HFHayhmwPOOyE7K34hOjbhuG8gizMFi1yj%2BX4CmQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAKB7vAJwAZT173V-HTtswhPE6Ng%2BPunoWW4VXSA%2B7%3D%3D1Db-%3DGA%40mail.gmail.com.

For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAErPVf2oGf92qX0L2egm%2B6qTgfMc7Bt8QDwkU%2ByWXOjgWJqOGw%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...