[MW:23935] Niobium in SA 516 GR 70 PLATE

Dear Experts ,

We intend to use SA 516 GR 70 plate - (thickness ranging from  55mm to 100 mm)  for   steam boiler application.
We are getting plates with Niobium content of 0.04 %.
As per SA 20   corresponding table ,the maximum limit for Nb  is 0.02 %
How ever , in the notes of the said Table  the Nb can be increased
What is effect of increase,  in Nb element on boiler drum shell rolling and  welding


--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/05cb8aec-9be2-45e2-8d97-57c1b2dae3b7%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...