Tuesday, November 24, 2015

[MW:23909] Bulge P-91 Pipe after PWHT

Dear Expert,
In P91 Material ( HRSG header Joint ) after pwht one joint is bulge.We did  Preheating ,Welding , Post Heating,& PWHT in proper way.
Can anybody explain why this bulge occurs & remedy.
During fit-up inspection & weld visual inspection all round the joint is perfect but after PWHT pipe is bulge 140 mm away from the   weld ment
Pic Attached
Regards,
Pradip

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAB%3DAs8kfusRiywON4c0YxkK74WcPtsqTEFnp9QH-4KyzX%2BrSrA%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...