Sa2.5 is a blast finish by definition and is achievable only by blasting with grit or other blast media. This equipment may claim to produce a finish equivalent to Sa2.5 but most clients will not accept it.

 

Alan Denney

AKD Materials Consulting Ltd

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Madhan S
Sent: 22 November 2015 04:51
To: Materials & Welding <materials-welding@googlegroups.com>
Subject: [MW:23907] Re: S.A. 2.5 surface profile

 

You can also use bristle blaster machine to achieve SA 2.5 finish for weld joints, touch up and repair areas. But it is a slow process.

 

Check the attached document.

 


On Tuesday, August 18, 2015 at 10:04:06 AM UTC+3, Jasim Ahmed wrote:

Dear experts,

 

I badly need to know - is it possible to create S.A. 2.5 surface profile for joint wrapping without sand blasting?

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/38a30053-9679-4b69-baa4-448d31c24b0d%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...