Friday, November 20, 2015

[MW:23904] RE: 23898] MAGNETIC PARTICLE AND LIQUID PENETRANT EXAMINATION

It would help us to give some guidance if you could inform us what industry you work in or what components you are interested in. The question is rather too open-ended.

 

Alan Denney

AKD Materials Consulting Ltd

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Tim Lim
Sent: 18 November 2015 12:18
To: Materials & Welding <materials-welding@googlegroups.com>
Subject: [MW:23898] MAGNETIC PARTICLE AND LIQUID PENETRANT EXAMINATION

 

Dear Esteem Colleagues,

 

I would like as much feedback as possible regarding when and where test for surface defects such as PT or MT is normally specified. My question is directed at design situations that dictate such choice of examination rather than nature of the construction.

 

Best regards,

Tim

 

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/38628ad6-688a-4d55-9657-199b78970610%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35737] Bend Test and Tensile Test failed for ET45 Micro Welded Coupon

Hi As its %elongation is very low  Better try buttering on jt surrace with ductile consumable like pure Ni i. E Ni1 And later weld jt with c...