[MW:23902] Re: Other Project PQR Can be used New project on Different Clients?

Please refer QW-201 Manufacturer's or Contractor's Responsibility (ASME IX - 2011) .It solves your query.

Thanks,
Sundar 

On Thursday, November 19, 2015 at 6:50:01 AM UTC+3, dominic v.k.dominic wrote:
Dear Expertise,
The contractor submitted other project PQR and approved by some other third party company and client.
My Question: Can used other client approved PQR for this new project and new Client?
In the code (API-1104 and ASME Section -IX) anywhere specified in this matter for Employer can be used other project PQR-If matching According the codes and new client requirements.
If yes, please provide code reference.

Thanks in Advance.
Best Regards,
Dominic.



--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/9129bd1f-1407-46f3-9799-5f1c37e5fc94%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...