As per AWS D 1.1 Clause No 5.22.4.3 correction is allowed in root openings.

1) Shall we conduct  WPS for buttering?
2) What tests to be carried out to qualify the WPS?

--
Thanks & Regds,

Prashant  Pansare
Cell no - 09987189854

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAFw%3DPEgxGOR-7ULXmnr0ctQt-ZZE%3Ds_ozekFMpaDqCU1JUS_zQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...