Gents,
 
Please guide in consumable selection to weld C276 Pipes to B462 Fittings and also what additional testing's are required (Beyond Sec IX testing's). This requirement if for H2SO4 plant piping
 
Regards
Raghava

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.