Re: [MW:23503] Governing Thickness for PWHT(B31.1&31.3)

For one more time I recommend to read all the relevant chapter of the Code and not isolated paragraphs.
So I would like to draw your attention also to the following paragraphs
132.1.2
132.2 (B)
and to 132.4.2

best regards

Dr. Georgios Dilintas