Hi ,

 I am looking for WRC Bulletin No 350 - Design Criteria for Dissimilar Metal Welds
.

 If somebody has , please can share it .

Regards,

On Tue, Sep 15, 2015 at 7:04 AM, Kadir godil <kadirgodil@gmail.com> wrote:
Dear experts,

I wanted to know, if someone has cross verified and calculated the Impact energy shown by Charpy/Izod impact test machine?

Please share the calculation method if someone has.

Thank you

Sincerely,
Abdulkadir

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/64940184-17ce-4f5b-9206-b29c09f4d9c3%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAKWVd7X7x5ntmw9kHbz3_54_YJtSPYH1oQ63yUA5pi2%3DVr6AqQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35374] Material Certification 3.1 / 3.2/2.2--EIL India

Dear Perumal, I answer the same but got one more question where it is written that TPI witness is mandatory? -- https://materials-...