Re: [MW:23468] Piping WPS/PQR and Welder Qualification Compliance- ASME IX or ASME B31.3

follow construction code  in addition to sec 9

THANKS & BEST REGARDS,
KG.PANDITHAN, IWE,  AWS-CWI, CSWIP 3.1,
CONSULTANT-WELDING & QUALITY

On Sun, Sep 13, 2015 at 2:53 AM, Anban <gane2478@hotmail.sg> wrote:
Dear Sirs
Appreciate if you could provide clear and definitive response.

In my Yard Piping WPS/PQRs and Welders Qualification comply with ASME IX only.

ASME IX specifically developed as  Qualification Standard for Welding,Brazing, and Fusing Procedures;Welders; Brazers; and Welding,Brazing, and Fusing Operators
ASME B31.3- ASME Code for Process Piping.- (Design/Construction Code)


As For Welder/Operator/Brazer Qualification& Piping WPS/PQR Qualifications- what is mandatory code- ASME IX or Design/Construction Code ASME B31.3?


For example High Pressure Piping ASME B31.3 Chapter IX shall be complied for WPS/PQRs and Welder Qualifications.
Yes, PWHT requirements one need to comply with ASME B31.3-Table 331.1.1

Does that mean ASME IX requirements superseded by ASME B31.3 Chapter IX?
Where and when one shall comply with ASME B31.3 instead of ASME IX.?


Thanks


--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/ecf4c1ee-a46c-4bd7-aec7-2ba942eaa094%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eOHHnEmNELBsXWKLjT934jeOYFSO%3DYwirA-JzMzBqJHiQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35614] Re: SS FILLER

dear , pl check A number and Gas composition use for ss cant be sutibale same % for duplex., u need to qualified with aditional testing of f...