Sunday, September 13, 2015

[MW:23470] QW-452.1 Note-2


Dear all,

question regarding the QW-452.1 note-2,

 "(2) Coupons tested by face and root bends shall be limited to weld deposit made by one welder with one or two
processes

Example  : W-62 with GTAW+SMAW Thk 10mm

 or two welders with one process each. 

Example W-61 & W-62 with GTAW+SMAW

Now,

"Weld deposit by each welder and each process shall be present
on the convex surface of the appropriate bent specimen."

how can SMAW shall be represent on convex surface ? i feel GTAW will always come since root welding had been done.

any idea??

or i misinterprete this clause?

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/bcaa058f-7f91-42b1-ade6-72ea8a39dcf5%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35597] INCONEL 825

Dear all  INCONEL 825 matching filler   ER NI FECR-1 its correct please guide me Regarding  Elavarasan -- https://materials-weldin...