Sunday, September 13, 2015

Re: [MW:23467] ASME B31.3-2010 Chapter IX- PQR Qualification- PWHT Min & Max Temperature allowed

check with MTC, and get  Tempering temperature, , PWHT should be below of 28 deg from base metal tempering  temp

THANKS & BEST REGARDS,
KG.PANDITHAN, IWE,  AWS-CWI, CSWIP 3.1,
CONSULTANT-WELDING & QUALITY

On Sun, Sep 13, 2015 at 3:57 AM, Anban <gane2478@hotmail.sg> wrote:

Dear Sirs
PQR qualified for ASTM A 519 Grade 4130-High Pressure Piping.
Test Coupon- 6.75" OD x 22.2mm
Weld Process - GTAW /GMAW
PWHT at 720 deg C
Base Material - Heat Treatment -Tempered Temp. at 1340F ( 726.7 deg C )

K331.1 General

K331.1.1 Heat Treatment Requirements.

The provisions of para. 331 and Table 331.1.1 apply, except as specified below.


 

(b) For welds other than longitudinal in quenched and tempered materials, when heat treatment is required by the engineering design, the temperature shall not be higher than 28°C (50°F) below the tempering temperature of the material.

       What does it really mean by stating- "shall not be higher than 28 deg C below Base Mat Tempering Temp " 698 deg C or 754 deg C?


Thanks

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/bb94d387-0702-4f1c-88c0-226cd029fbc4%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eOMCideDRQgx0xh7Ge6j3ReajirqSw-xg900JV4JPTWOg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...