As a professional you are required to use engineering judgement as well and read the code to you advantage. I understand the question to be can you use a welding procedure qualified on one consumable at minus 30 deg C to qualify where you are required to meet an impact requirement in the specification at minus 45 deg C. Regardless of what the code says this can hardly be considered a correct thing to do. Are you aware of the transition behaviour of steel and have you seen a catastrophic brittle fracture? If this is a pressure system or a structure seeing low temperatures you need to take care to ensure the product will not fail in a brittle way.

 

Alan Denney

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Anup N K E
Sent: 11 September 2015 15:41
To: materials-welding@googlegroups.com
Subject: Re: [MW:23459] WPS REVISION // Impact test temperature

 

Yes  the same PQR can be used. Please go through  QW 404.12 part e of Section IX.

Regards,

Anup

On 11 Sep 2015 06:50, "Raghuram Bathula" <raghurambathula@gmail.com> wrote:

No, you need to follow your code of construction and support with new PQR qualified at or below MDMT

 

On 11 September 2015 at 09:12, Mahesh Mirje <mahesh.mirje41@gmail.com> wrote:

Hi expert's,
I have PQR with electrode E7018, AND IMPACT tested at -30deg. Lets say Observed energy values 20J
Can I make wps with E7018-1, FOR IMPACT REQUIRMENT at -45 deg.required energy values 20j,
AS per ASME weld metal produced by 7018-1,  will provide 20j at -45 deg.
And HAZ ENERGY VALUES CAN BE CONTROLLED BY RESTRICTING HEAT INPUT.
Pls, clarify can I prepare wps for 7018-1 at -45 by restricting heat input as same used in 7018 PQR.

Regards
Mahesh

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADxVubnJSKpehomULf6bXi%2Bv0%2BuKQesPQX2vT8KNC_YYacnnhw%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJsQutYpcSXWVq8afZqf51DPjzznrojzQW9t1vfgwu5jtbMiCQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35354] Cast-iron welding

1. Preheat joint area(other area, cover with mineral wool). 2. ENiCi or ENiFe-CI. 3. stringer bead. 4. peening is to be done on weldmetal im...