Saturday, September 12, 2015

[MW:23462] Weld Metal Analysis of API 5L BMS PSL 2

Dear Experts,

I have one doubt.
We are receiving API 5L BMS PSL 2 welded pipes having the PMI report attached for Weld Metal.
My Question,
Does the chemical analysis (PMI) of Weld metal shall meet the acceptance criteria of same as base metal ?

I want to know the reference of the chemical analysis acceptance range for the welded part.

--
Thanks & Regards
Biplab Pal
Welding Inspector
E-mail:   biplab.mech@gmail.com
 
Information in this email and any attachments is confidential and intended solely for the use of the individual(s) to whom it is addressed or otherwise directed. Please note that any views or opinions presented in this email are solely those of the author and do not necessarily represent those of the Company. Finally, the recipient should check this email and any attachments for the presence of viruses. Myself accepts no liability for any damage caused by any virus transmitted by this email.
 

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAFnzQg0721r8%2BDejqgSh6yreUWPXa5vK4vs5%3DZdpamC%3D3PdmMQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35354] Cast-iron welding

1. Preheat joint area(other area, cover with mineral wool). 2. ENiCi or ENiFe-CI. 3. stringer bead. 4. peening is to be done on weldmetal im...