Friday, September 11, 2015

Re: [MW:23459] Welding consumables (2.25Cr-1Mo-0.25V) with guaranteed stress rupture strength

Hi

Do you need SRT according to ASME BPVC VIII div 2

540 deg 210 Mpa for 900 hour
Or

It also depends on the client requirement: Eg :chevron
538deg 207Mpa 1000 hour

Results are different for SRT

Regards

Shyamal das

Sent from my iPhone

> On Aug 27, 2015, at 6:54 AM, S.Mohammed <mohd52100@gmail.com> wrote:
>
> Expert opinion needed.
>
> --
> You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
> To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
> To post to this group, send email to materials-welding@googlegroups.com.
> Visit this group at http://groups.google.com/group/materials-welding.
> To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/27b7de07-9427-4e41-92b0-125ff396af62%40googlegroups.com.
> For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1AE54E3F-CE23-43EB-806F-FE6483EABB25%40gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...