Dear Sir,
Co relation of fittings class with pipe schedule is given in table 2 of ASME B16.11- FORGED FITTINGS, SOCKET-WELDING AND THREADED
Can we use the same to find the governing thickness with respect to the thickness qualified by the welder to weld the groove joint (olet to mother pipe) .
Regards,
Anup
On Thu, Sep 10, 2015 at 4:02 PM, <george.dilintas@gr.bureauveritas.com> wrote:
--You have to go to the design and construction Code and check what is the governing thickness
best regards
Dr. Georgios Dilintas
Authorized Nuclear Inspector
Authorized Inspector Supervisor
I&F REGIONAL TECHNICAL MANAGER
BUREAU VERITAS PIRAEUS - GREECE
Tel: +30 210 40 63 113 /4 /5
Fax: +30 210 40 63 118
Cell: +30 69 44 64 62 04
This message contains confidential information. To know more, please click on the following link: http://disclaimer.bureauveritas.com
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/OFBAD47D13.7F114A68-ONC2257EBC.00478FAF-C2257EBC.0047A2A8%40LocalDomain.
For more options, visit https://groups.google.com/d/optout.
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJsQutZgro6Ds3rtcRwc8r0DSqEx4zztA2heYy5JwX91FEoCvQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.
No comments:
Post a Comment