Do not confuse between base metal thickness (T) and deposited thickness (t)
best regards
Dr. Georgios Dilintas
Authorized Nuclear Inspector
Authorized Inspector Supervisor
I&F REGIONAL TECHNICAL MANAGER
BUREAU VERITAS PIRAEUS - GREECE
Tel: +30 210 40 63 113 /4 /5
Fax: +30 210 40 63 118
Cell: +30 69 44 64 62 04
Mahesh Mirje ---05/09/2015 20:07:28---Hi experts, I have two PQR'S
From: Mahesh Mirje <mahesh.mirje41@gmail.com>
To: Materials & Welding <materials-welding@googlegroups.com>
Date: 05/09/2015 20:07
Subject: [MW:23398] Difference between QW-200.2(f) and 200.4(b)
Sent by: materials-welding@googlegroups.com
Hi experts,
I have two PQR'S
1) GTAW : PROVIDES BASE METAL RANGE 1.5 TO 5
2)SMAW : PROVIDES BASR METAL RANGE 5 TO 32
QUESTION : CAN I MAKE WPS QUALIFICATIONS RANGES FROM 1.5 TO 32
AS PER QW200.2(f): yes
As per QW 200.4(b): No
Also refer interpretation IX-10-34
I stuck between these two clauses and interpretation,
Can any one provide correct interpretation.
Thanks
Mahesh mirje
--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/667d22f6-242a-4907-8949-453aac804d44%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.
This message contains confidential information. To know more, please click on the following link: http://disclaimer.bureauveritas.com
No comments:
Post a Comment