Dear Experts,

Can anyone answer this concern.


We have WPS & PQR for piping, qualified with GTAW + SMAW. Now we indent to do backchip for the production joints. Does this asks for requalification of PQR. Is this a essential variable. Where it is address in QW- 256 & QW-253.

Please advice.

cordially,
Jay Poojary

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAAcO%3DySNJmLAuLRy5_mVXsZO7utO-eHekKxE8T3B4wr5or%2BxsQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...