Re: [MW:23472] Piping WPS/PQR and Welder Qualification Compliance- ASME IX or ASME B31.3

Design and construction Code requirements have  prevalence

Sent from my BlackBerry 10 smartphone.
From: Anban
Sent: Κυριακή, 13 Σεπτεμβρίου 2015 - 07:24
To: Materials & Welding
Reply To: materials-welding@googlegroups.com
Subject: [MW:23463] Piping WPS/PQR and Welder Qualification Compliance- ASME IX or ASME B31.3

Dear Sirs
Appreciate if you could provide clear and definitive response.

In my Yard Piping WPS/PQRs and Welders Qualification comply with ASME IX only.

ASME IX specifically developed as  Qualification Standard for Welding,Brazing, and Fusing Procedures;Welders; Brazers; and Welding,Brazing, and Fusing Operators
ASME B31.3- ASME Code for Process Piping.- (Design/Construction Code)


As For Welder/Operator/Brazer Qualification& Piping WPS/PQR Qualifications- what is mandatory code- ASME IX or Design/Construction Code ASME B31.3?


For example High Pressure Piping ASME B31.3 Chapter IX shall be complied for WPS/PQRs and Welder Qualifications.
Yes, PWHT requirements one need to comply with ASME B31.3-Table 331.1.1

Does that mean ASME IX requirements superseded by ASME B31.3 Chapter IX?
Where and when one shall comply with ASME B31.3 instead of ASME IX.?


Thanks


--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/ecf4c1ee-a46c-4bd7-aec7-2ba942eaa094%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

This message contains confidential information. To know more, please click on the following link: http://disclaimer.bureauveritas.com

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...