Thursday, September 10, 2015

[MW:23432] Re: Welding consumables (2.25Cr-1Mo-0.25V) with guaranteed stress rupture strength

D&H Secheron make Cromotherme 2V(MOD).
Technical leaflet is enclosed.
You may be sent further query on following mail ID
vinay.tripathi@dnhsecheron.net/tjprao@dnhsecheron.net

Thanks
Vinay Tripathi


On Tuesday, March 9, 2010 at 5:08:53 PM UTC+5:30, Bathula Raghuram (Mumbai - PIPING) wrote:

Can anybody suggest the consumable brands/mfr name who can give guaranteed results (if possible pl. attach data sheet)  for high temperature Stress Rupture testing of all batches of welding consumables used at 1000°F & 30ksi stress. The time of failure shall exceed 900 hrs.

Thanks in adv.


--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/64312b10-ad7d-4bb9-bd4f-97ad989e1210%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...