Agree with the answer from denney. It's all depends on the designer's response to approve your request.
在2015年09月09日 22:24,Alan Denney 写道:
I have known this sort of concession request to be granted and also, in other cases to be rejected. It depends on many factors in the situation. The testing performed would be different, but that may not be seen as critical. All you can do is to make the case to your client and await their response.
Alan Denney
AKD Materials Consulting Ltd
-----Original Message-----
From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of mohd firdaus
Sent: 09 September 2015 14:08
To: materials-welding@googlegroups.com
Subject: [MW:23425] Using ASME IX WPS for replace with AWS D1.1 structure job
Dear all,
I have a situation here. We got steel structure job but my AWS D1.1 WPS not covered for this job. It is possible to replace the WPS WITH ASME IX WPS?. My boss told me to sent the STQ request for replace the AWS D1.1 to ASME IX. I don't have any idea for this. Please guide me. Thank you.
Mohd Firdaus Abd Rahim
QA/QC
+60122796361
Sent from my iPhone
--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CEC1A20B-5BC3-4448-A2D6-60067EA848D2%40gmail.com.
For more options, visit https://groups.google.com/d/optout.
This email has been scanned by BullGuard antivirus protection.
For more info visit www.bullguard.com
--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/001301d0eb0a%24c477a4c0%244d66ee40%24%40denney1.freeserve.co.uk.
For more options, visit https://groups.google.com/d/optout.
No comments:
Post a Comment