Hi All,

 

We use 100% Argon as a shielding gas when welding our super duplex stainless steel, we use Tig welding on our tube mills. We then hydro form these tubes, but find that weld failures are more prevalent with the super duplex stainless steels than with the other stainless steels we weld (i.e. 316, 312, etc).

 

Does anyone have any suggestions. Is there anything different we need to do when welding the super duplex stainless steel?

 

Regards,

 

Naasief

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Noe Mota
Sent: 18 November 2014 07:44 PM
To: materials-welding@googlegroups.com
Subject: Re: [MW:22286] Compare Argon with Nitrogen as Purging gas for Super duplex stainless steels

 

The best approach for gas purging when welding super duplex is argon 100%.

El nov 16, 2014 9:56 p.m., "Murugesan Jeyaraman" <jmurugesan@gmail.com> escribió:

Dear All 

 

Which gas is better for purging gas of super duplex stainless steel welds. 

 

Please compare both technically, also suggest which is best to use in Duplex SS purging?  Is there any difference at all or both just gives equal result?

 

--

Thanks and Regards

 

Murugesan 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.




This email has been scanned for email related threats and delivered safely by Mimecast.
For more information please visit http://www.mimecast.com

No comments:

[MW:35725] Dismillar material Welding

Dear experts,  In my Hydro Electric Project  materials using A517Gr.F and A537CL-II.  For A517Gr.F using E 11018M and A537CL-II using E 9018...