Monday, November 17, 2014

RE: [MW:22279] Compare Argon with Nitrogen as Purging gas for Super duplex stainless steels

Hi Ahmad,

 

Does using this combination of shielding gas (Argon and Nitrogen) have any influence on the weld strength (i.e. integrity of the weld), when welding super duplex stainless steels.

 

Regards,

 

Naasief

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Ahmad el-sharkawy
Sent: 17 November 2014 01:16 PM
To: materials-welding@googlegroups.com
Subject: Re: [MW:22277] Compare Argon with Nitrogen as Purging gas for Super duplex stainless steels

 

use mix of nitrogen and argon
 (Ar + 1 -2%N2 as a shielding gas)




 

On Mon, Nov 17, 2014 at 2:56 AM, Murugesan Jeyaraman <jmurugesan@gmail.com> wrote:

Dear All 

 

Which gas is better for purging gas of super duplex stainless steel welds. 

 

Please compare both technically, also suggest which is best to use in Duplex SS purging?  Is there any difference at all or both just gives equal result?

 

--

Thanks and Regards

 

Murugesan 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.




--

WITH MY BEST WISHES

AHMED ELSHARKAWY
QA/QC ENGINEER
DIPLOMA DEGREE IN WELDING ENGINEERING.
CERTIFIED WELDING INSPECTOR " CWI "
14072901.
ASNT LEVEL II "
RT&VT&UT&PT&MT"
IRECA CERTIFIED LEAD EDITOR ISO 9001/2008.

PREPARING MASTER DEGREE IN WELDING ENGINEERING.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.




This email has been scanned for email related threats and delivered safely by Mimecast.
For more information please visit http://www.mimecast.com

No comments:

Re: [MW:35354] Cast-iron welding

1. Preheat joint area(other area, cover with mineral wool). 2. ENiCi or ENiFe-CI. 3. stringer bead. 4. peening is to be done on weldmetal im...