Dear All,
 
Can anyone tell me What is the minimum gauge range difference in a pressure testing?

 

Let me explain clearly, now my hydro test pressure is 10 bar. As per ASME Sec VIII Div 1 UG-102 TEST GAGES and ASME Sec V ARTICLE 10 LEAK TESTING T-1030 EQUIPMENT I can use pressure gauge range 1.5 to 4 times of the test pressure i.e. 0-15 Bar to 0-40 barg.

 

Now my question is can I use these both the gauges (0-15 Bar to 0-40 barg) in a single pressure? If yes please give me code reference.

 

There is an argument saying that the "minimum of two pressure gauges shall be within 5 % of one another when in use"

 

 

Thanks in advance.

 

Regards,

Santosh.

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35748] Re: PQR- Chemical testing requirements

As answered by everyone, chemical is not required. Notwithstanding, please note that A-No. which denotes weld metal chemical composition is ...