SA is an ASME specification for the analysis of ferrous materials. A387 / A387M are the specification number for that particular material. 06a is the year when it was approved by ASME. While 'P" is the number assigned to that material because of its properties. the numerical figure 91 attributes the composition of elements it contains. I found the regarding info in www.weldpedia.com

On Friday, October 17, 2014 11:40:41 AM UTC+5, Akhilesh singh wrote:
Plz help me regarding such full-form:

1. ASME full form of SA - A 387/A 387M – 06a ............. what does means of "SA" - "A" 387 ................. "A387M" - "06a"..........................???

                          or
             A 387/A 387M – 06a

2. Grade P91 steel (A 387/A 387M – 06a)
    what does me "P"  & "91"

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35737] Bend Test and Tensile Test failed for ET45 Micro Welded Coupon

Hi As its %elongation is very low  Better try buttering on jt surrace with ductile consumable like pure Ni i. E Ni1 And later weld jt with c...