Dear All,
Kindly suggest FCAW consumable for SS410 And IS2062 MS dissimilar joint.
also how does Nickel affect in dissimilar joint and what Ni percentage generally required for dissimilar joint.
E309Lt1 can be used for SS410&MS IS2062 Joint?
Regards
Raj
-- Kindly suggest FCAW consumable for SS410 And IS2062 MS dissimilar joint.
also how does Nickel affect in dissimilar joint and what Ni percentage generally required for dissimilar joint.
E309Lt1 can be used for SS410&MS IS2062 Joint?
Regards
Raj
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.
Comments