RE: RE: [MW:20125] Combination PQR to one WPS

I have given you the relevant ASME Section IX paragraph citations in my previous response.

 

You might also want to look at ASME Interpretation IX-10-34. 

 

 

I believe that this more complex question, addresses your question.

 

John A. Henning

Welding & Materials

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of venkateswaran k
Sent: Monday, February 17, 2014 2:59 AM
To: materials-welding@googlegroups.com
Subject: Re: RE: [MW:20120] Combination PQR to one WPS

 

Mr.John

can you refer me the standard that mentioned this thickness limit for GTAW

Regards


On Mon, 17 Feb 2014 11:14:15 +0530 wrote
>NO - GTAW is not qualified to weld any base metal thicker than 11mm.





-----Original Message-----

From: materials-welding@googlegroups.com on behalf of Ali Samdani

Sent: Fri 2/14/2014 11:41 PM

To: materials-welding@googlegroups.com

Subject: Re: [MW:20106] Combination PQR to one WPS



Just in case if I specify in my WPS that I'll use GTAW process for root

pass only and SMAW process for fill passes. Keeping in view SMAW process

qualification range (up to 14.22 mm), will my WPS qualification range not

up to 14.22 mm?



Regards,





On Thu, Feb 13, 2014 at 7:35 PM, John Henning wrote:



> The answers you have received are correct but somewhat incomplete.

>

>

>

> If you are going to combine PQR's to make a single WPS, the essential

> variables for each process must be met - see QW-200.4. Qualified base

> metal thickness is an essential variable and is determined from QW-451.1

> and PQR base metal thickness. From QW-451.1, for your example, each

> process is limited to base metal thickness range of 1.5mm to 2T. Thus,

> your GTAW process is limited to a maximum base metal thickness of

> 2*(5.54mm) or 11.08mm while the SMAW process is qualified for welding base

> metal thickness up to 14.22mm. The base metal thickness range for the GTAW

> process is the limiting condition. If a combined WPS is written from

> these two PQRs, your qualified base metal thickness range is: 1.5mm *<*T

> *

> since GTAW is not qualified to weld any base metal thickness greater than

> 11mm.

>

>

>

> I hope this makes the issue more clear.

>

>

>

> John A. Henning

>

> Welding & Materials

>

>

>

> *From:* materials-welding@googlegroups.com [mailto:

> materials-welding@googlegroups.com] *On Behalf Of *veera raghava

> kommisetti

> *Sent:* Thursday, February 13, 2014 6:06 AM

> *To:* materials-welding@googlegroups.com

> *Subject:* Re: [MW:20090] Combination PQR to one WPS

>

>

>

> No

>

>

>

> On Thu, Feb 13, 2014 at 10:46 AM, Original Man wrote:

>

> Back ground: One Welding procedure was qualified with GTAW process with

> base material thickness 5.54 mm with material API 5L Gr.B And Another

> was qualified with SMAW process with base material thickness 7.11 mm

>

> Question: May this both PQR support a WPS with GTAW + SMAW process for

> the base material thickness from 14 mm for the same material and same

> variables ?

>

> --

> To post to this group, send email to materials-welding@googlegroups.com

> To unsubscribe from this group, send email to

> materials-welding+unsubscribe@googlegroups.com

> For more options, visit this group's bolg at

> http://materials-welding.blogspot.com/

>

> http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm

>

> The views expressed/exchnaged in this group are members personel views and

> meant for educational purposes only, Users must take their own decisions

> w.r.t. applicable code/standard/contract documents.

> ---

> You received this message because you are subscribed to the Google Groups

> "Materials & Welding" group.

> To unsubscribe from this group and stop receiving emails from it, send an

> email to materials-welding+unsubscribe@googlegroups.com.

> For more options, visit https://groups.google.com/groups/opt_out.

>

>

>

> --

> To post to this group, send email to materials-welding@googlegroups.com

> To unsubscribe from this group, send email to

> materials-welding+unsubscribe@googlegroups.com

> For more options, visit this group's bolg at

> http://materials-welding.blogspot.com/

>

> http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm

>

> The views expressed/exchnaged in this group are members personel views and

> meant for educational purposes only, Users must take their own decisions

> w.r.t. applicable code/standard/contract documents.

> ---

> You received this message because you are subscribed to the Google Groups

> "Materials & Welding" group.

> To unsubscribe from this group and stop receiving emails from it, send an

> email to materials-welding+unsubscribe@googlegroups.com.

> For more options, visit https://groups.google.com/groups/opt_out.

>

> ______________________________________________________________________

> The information in this email is confidential, and is intended solely for

> the addressee(s). If you are not the intended recipient of this email

> please let us know by reply and then delete it from your system; you should

> not copy this message or disclose its contents to anyone. The internet can

> not guarantee the integrity of this message. HAMON (and its subsidiaries)

> shall (will) not therefore be liable for the message if modified.

> ______________________________________________________________________

>

> --

> To post to this group, send email to materials-welding@googlegroups.com

> To unsubscribe from this group, send email to

> materials-welding+unsubscribe@googlegroups.com

> For more options, visit this group's bolg at

> http://materials-welding.blogspot.com/

>

> http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm

>

> The views expressed/exchnaged in this group are members personel views and

> meant for educational purposes only, Users must take their own decisions

> w.r.t. applicable code/standard/contract documents.

> ---

> You received this message because you are subscribed to the Google Groups

> "Materials & Welding" group.

> To unsubscribe from this group and stop receiving emails from it, send an

> email to materials-welding+unsubscribe@googlegroups.com.

> For more options, visit https://groups.google.com/groups/opt_out.

>



--

To post to this group, send email to materials-welding@googlegroups.com

To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com

For more options, visit this group's bolg at http://materials-welding.blogspot.com/

http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm



The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

---

You received this message because you are subscribed to the Google Groups "Materials & Welding" group.

To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.

For more options, visit https://groups.google.com/groups/opt_out.





______________________________________________________________________

The information in this email is confidential, and is intended solely for the addressee(s). If you are not the intended recipient of this email please let us know by reply and then delete it from your system; you should not copy this message or disclose its contents to anyone. The internet can not guarantee the integrity of this message. HAMON (and its subsidiaries) shall (will) not therefore be liable for the message if modified.

______________________________________________________________________



--

To post to this group, send email to materials-welding@googlegroups.com

To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com

For more options, visit this group's bolg at http://materials-welding.blogspot.com/

http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm



The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

---

You received this message because you are subscribed to the Google Groups "Materials & Welding" group.

To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.

For more options, visit https://groups.google.com/groups/opt_out.

 

Get your own FREE website, FREE domain & FREE mobile app with Company email.  

Know More >

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.


______________________________________________________________________
The information in this email is confidential, and is intended solely for the addressee(s). If you are not the intended recipient of this email please let us know by reply and then delete it from your system; you should not copy this message or disclose its contents to anyone. The internet can not guarantee the integrity of this message. HAMON (and its subsidiaries) shall (will) not therefore be liable for the message if modified.
______________________________________________________________________

Comments

Popular posts from this blog

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...

[MW:5202] RE: 5200] NDT after PWHT

------------------------------------- Interpretation:  I‑89‑14 Subject:         Section I (1986 Edition, 1987 Addenda), PW‑11,                  NDE Prior to PWHT Date Issued:     December 15, 1988 File:            BC88‑393   Question: Does PW‑11 require that NDE be performed on welds after they have been subjected to the postweld heat treatment required by PW‑39?   Reply: No, unless the conditions described in PW‑11.2.2 exist. ---------------------------------------------- Interpretation:  VIII-1-98-09 Subject:         Section VIII, Division 1 (1995 Edition, 1996 Addenda); NDE                 ...

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...