Skip to main content

Re: [MW:20146] MPT test method to check the Lamination on the Bevel Edge.

best to go with DPT


On Wed, Feb 19, 2014 at 8:37 PM, Shashank Vagal <nach_sam@yahoo.com> wrote:
MB,
VT & PT - that's all you need
 
With Best Regards,
Shashank C Vagal 


On Wednesday, 19 February 2014 4:31 PM, MK Sethu <scorpiosethu@gmail.com> wrote:
Which probe is to be used for lamination check in pipe bevel. Kindly explain how to do inside or outside the pipe

Thanks and regards

MK Sethu

On Tuesday, September 18, 2012 12:17:14 PM UTC+1, muthu barathi wrote:

You have to mention some more details for correct advice.

1. whether the bevel was made by gas cut or machining?
If gas cut used w, while gas cutting it might be opened if lamination was present.

AC will detect only surface not sub surface.
If you want to see sub surface defects then you have to go for HWDC. That also you can go up
to 3mm effectively.
On Mon, 17 Sep 2012 21:36:56 +0530 wrote
>Dear Exparts,
 
I have a doubt regarding MPT method.
I am going to check the lamination of plates from the bevel edges.
What MPT current mode should we use.
Is it AC or HWDC?
Please share your knowledge and code references.
 
--


Thanks & Regards
Biplab Pal
Welding Inspector
E-mail:   bipla...@gmail.com
 
Information in this email and any attachments is confidential and intended solely for the use
of the individual(s) to whom it is addressed or otherwise directed. Please note that any views
or opinions presented in this email are solely those of the author and do not necessarily
represent those of the Company. Finally, the recipient should check this email and any
attachments for the presence of viruses. Myself accepts no liability for any damage caused by
any virus transmitted by this email.

 




--
>
To post to this group, send email to material...@ googlegroups.com
>
To unsubscribe from this group, send email to materials-weld...@ googlegroups.com
>
For more options, visit this group's bolg at http://materials-welding. blogspot.com/
>
http://www.linkedin.com/ groups/MaterialsWelding- 122787?home=&gid=122787&trk= anet_ug_hm
>

>
The views expressed/exchnaged in this group are members personel views and meant for
educational purposes only, Users must take their own decisions w.r.t. applicable
code/standard/contract documents.
>

>

>


Dear Sir,





Thanking You.

With Warm Regards,

Muthu barathi P,
Mobile No. 9099006785

Follow Rediff Deal ho jaye! to get exciting offers in your city everyday.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.



--
DINESH VITTHAL SOMWANSHI

BACHELOR IN MECHANICAL ENGINEER
AUTHORIZED WELDING / NDT / PAINTING INSPECTION PERSONNEL,
AWS - CWI , CSWIP 3.1
BGAS  Gr 2 / 3
NDT II -UT , RT , MT , PT, VT

Pray for others, sometime, You might never need to pray for yourself again.....

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...