Hi
 
Rudolf is correct.
As per ASME Sec IX, Only thing you need to check is that the welder has welded the particular process for which he was qualified in the last six months and maintain the Welder Continuity Record for the same.
 
Regards
 
Prem Nautiyal
cell: 9769316004
 


On Thursday, January 30, 2014 1:12 PM, Kumar <sk7920541@gmail.com> wrote:
Dear all
This means if the welder has performed in the particular processes irrespective of the positions and configurations, his qualifications can be considered as renewed..I think.. (ie..welder had qualified for 6g but done 1g sometimes in 6 month..but still he can be renewed for 6g..) kindly confirm
Thanks in advance,
Kumar.
On Jan 30, 2014 11:24 AM, "veera raghava kommisetti" <kommisetti@gmail.com> wrote:
Only Process matters.. Not weld configuration.


On Wed, Jan 29, 2014 at 3:58 PM, gulrez alam <gulrezhhi@gmail.com> wrote:
Dear experts

Can you explain to me .if any welder is qualified 6 month before with 2 " pipe .but this 6 month the welder is doing only fillet weld .

so i want to know this welder qualification is renew on his continue welding or need to retest.


Best regards 

G.Alam
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to mailto:materials-welding%2Bunsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to mailto:materials-welding%2Bunsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to mailto:materials-welding%2Bunsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to mailto:materials-welding%2Bunsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.


No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...