Thursday, January 30, 2014

Re: [MW:19957] RE: 19922] Writing multiple WPSs using single PQR for different processes in AWS D1.1

See file attachment.

For more interpretation:  http://www.aws.org/technical/interps/Subject.html

Em 27/01/2014 21:43, "John Henning" <jhenning@deltak.com> escreveu:

No.

 

See an old AWS D1.1 interpretation, I-9/91-10-03, to whit:

“Inquiry 1 – Can one or more welding process be deleted from a qualified welding procedure in accordance with AWS D1.1 Section 5.5, if each of the essential variables for each of the remaining processes  is maintained?  . . .

Reply 1 – No.  . . . “

 

Note section number will not agree with current edition – this was written before D1.1 was reorganized.  However intent is clear.

 

John A. Henning

Welding & Materials

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Pradip Patil
Sent: Thursday, January 23, 2014 8:15 PM
To: materials-welding@googlegroups.com
Subject: [MW:19922] Writing multiple WPSs using single PQR for different processes in AWS D1.1

 

Hi,

 

I have a query regarding AWS D1.1, Does it allow to write separate WPS for the processes qualified on PQR for GTAW + FCAW as like ASME Sec IX?

 

Can you share the clause number too.

 

While does any of AWS spec gives guidelines for Inconel 625 Weld overlay for structural parts?

 

With Regards,

 

Pradip.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.


______________________________________________________________________
The information in this email is confidential, and is intended solely for the addressee(s). If you are not the intended recipient of this email please let us know by reply and then delete it from your system; you should not copy this message or disclose its contents to anyone. The internet can not guarantee the integrity of this message. HAMON (and its subsidiaries) shall (will) not therefore be liable for the message if modified.
______________________________________________________________________

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...