Hi,

Since copper is having high thermal conductivity so to weld copper,
one should focus on preheating appox 300 to 400 degree C.

Also try to use optimum electrode/filler diameter to have more arc heat.

In copper premature cooling is always a problem.


Regards,

Zakir Ali.


From: Ganesh Mahankal <mahankalga@gmail.com>
Sent: Wed, 22 Jan 2014 18:24:43
To: materials-welding@googlegroups.com
Subject: [MW:19905] Copper Welding
Dear Sir ,
 
Preheating is very very important for copper welding.
also use dia 1.6 mm filler wire only for thickness less than 3 mm.
 
Best Regards,
Ganesh Mahankal
Alfa Laval India Ltd
+91 9970357971
 
 

On Friday, November 29, 2013 2:46:36 PM UTC+5:30, Avis wrote:
Dear All,
 
Anybody having experience is copper welding.  If yes please share your difficultites, and also welder availablity for the welding.
 
The base materials is ASTM B42 UNS C12200 (Cu - 99.9%)

P. No. is 31, SFA  - A5.7, F. No. 31.

Filler Wire Class - ER Cu Sn 1

With regards,
S. Sivasubramanian, Kuwait.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

Get your own FREE website, FREE domain & FREE mobile app with Company email.  
Know More >

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...