Thursday, January 23, 2014

Re: [MW:19913] % Ovality tolerance of A106 seamless pipe

Pl. refer ASTM A530 ( General Requirements for Specialized Carbon and Alloy Steel Pipe).

Regards 
G.S.Arora 
Ph: 91-7567125331


On Thursday, 23 January 2014 5:44 AM, Vairamuthu Ramar <vairamuthu78@hotmail.com> wrote:

 hi,
 
pls find the attached file for pipe ovality tolerance.
 
hope it will help you.
 
 

Date: Tue, 21 Jan 2014 20:54:18 -0800
From: pat.freedom072@gmail.com
To: materials-welding@googlegroups.com
Subject: [MW:19903] % Ovality tolerance of A106 seamless pipe

I'd like to know the % of ovality tolerance of CS pipe A106 seamless; 8" Sch.STD. Could you please someone can help?
 
Thanks & regards,
 
Pat

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.


No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...