Re: [MW:19910] Re: Thikness qualification for Tube to Tube sheet mock-up.

Mockup itself is not mandatory....


On Wed, Jan 22, 2014 at 4:40 PM, Ganesh Mahankal <mahankalga@gmail.com> wrote:
Dear Hemant ,
 
Plz go with 45 mm thick tube plate thickness.tube sheet thickness is not a essential variable.it should not be greater than 50 mm.
Plz take care of expansion groove. it should be covered into tubesheet thickness.
 
Best regards,

Ganesh Mahankal


PEM -Welding
Tel direct: +91 20 27107 664 - Mobile: +91 9970357971

ganesh.mahankal@alfalaval.com
Contact me on MS Lync/Communicator:
sip:ganesh.mahankal@alfalaval.com

Alfa Laval (India) Limited

Mumbai-Pune Road, Dapodi Pune - 411 012 Pune, Maharashtra - India
Registered Office: Mumbai Pune Road Dapodi Pune 411 012

 
 

On Monday, December 9, 2013 3:14:16 PM UTC+5:30, HEMANT SUTHAR wrote:

Dear Experts,

I have two Heat exchanger which same Tube sheet configuration Like tube hole PCD, Hole dia, Tube OD, Tube thickness, Weld design except Tube sheet thikness. My one job Thickness is 35 mm and second one is 45 mm.

Now pls suggest me for following points,

1.       Can I use one mock-up for both Heat exchanger?

2.       If I yes, which thickness I have to select?

 

 

Regards

Hemant H suthar

Asst. Manager QA/QC

Chemithon Engineers Pvt Ltd.

Khanvel-Kheradi Road. Silvassa, UT of DNH

Website: www.chemithon.co.in

Office Contact: 0260 2677889 / 2677036 , 37 Cell : 9712973092

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

No comments:

[MW:35738] ASME IX WPS Qualification Query: GTAW + FCAW with Multiple PQRs

Dear Welding Experts, I'm currently preparing a Welding Procedure Specification (WPS) and have encountered a request to qualify a GTAW +...