Friday, January 24, 2014

[MW:19922] Writing multiple WPSs using single PQR for different processes in AWS D1.1

Hi,


I have a query regarding AWS D1.1, Does it allow to write separate WPS for the processes qualified on PQR for GTAW + FCAW as like ASME Sec IX?

 

Can you share the clause number too.

 

While does any of AWS spec gives guidelines for Inconel 625 Weld overlay for structural parts?

 

With Regards,


Pradip.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...