Friday, January 17, 2014

[MW:19876] Re: Welding UNS S31254 to UNS S31254

Dear All,

ER NiCrMo-3 result are dood for lower thickness but for higher thickness i am getting problem. I am welding 10-16 mm thick plates please guide welding parameters for the same.

On Friday, November 15, 2013 3:28:52 PM UTC+5:30, prabhu wrote:
Dear All,

Can you guide me for selecting TIG filler wire for SMO 254  UNS S31254  to  UNS S31254 plate thickness 10mm
and in preparing WPS for same with parameters inputs.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...