A297 HD is a heat resistant casting alloy with 28Cr/5Ni.
I assume that in your project, welding of CS to A297 HD is for
structural purpose (welding supporting structure to casing etc). If it
is so, use E309L electrode and you will be fine.
If it is not a structural joint then please give us more information
about the service requirements.
Regards
Ramin Kondori
On 6/3/13, skroy <sanjeev.roy@fivesgroup.com> wrote:
>
>
>
>
>
>
>
>
>
>
>
>
>
> dear all
>
> can you suggest suitable welding filler wire or electrode for welding of
> carbon steel (A106 Gr.B) and ASTM A297 HD material.
>
> thanks
> with regards
>
> --
>
>
>
>
>
>
>
>
> *Sanjeev Kumar Roy*
>
> Manager - QA/QC, BFC
>
> *Fives Combustion Systems Private Ltd.*
>
> Plot No- 230, Padra Jambusar Highway, Dabhasa
>
> Vadodara, Gujarat, 391440* - India*
>
> Tel: +91 2662 308208 - Fax: +91 2662 308222
>
>
> sanjeev.roy@fivesgroup.com <mailto:sanjeev.roy@fivesgroup.com>
>
> www.fivesgroup.com <http://www.fivesgroup.com/>
>
> Fives on Youtube <http://www.youtube.com/groupfives>
>
>
>
>
> *This message and any attachments are confidential and for the sole
> attention of the addressees. Any unauthorized use or dissemination is
> prohibited.*
> Ce message et toutes pièces jointes sont confidentiels et à l'attention
> exclusive de ses destinataires.Toute utilisation ou diffusion non
> autorisée est interdite.
> *Please think about the environment before printing this e-mail.*//
> Merci de penser à l'environnement avant d'imprimer cet e-mail.
>
>
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to
> materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg at
> http://materials-welding.blogspot.com/
> http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
>
> The views expressed/exchnaged in this group are members personel views and
> meant for educational purposes only, Users must take their own decisions
> w.r.t. applicable code/standard/contract documents.
> ---
> You received this message because you are subscribed to the Google Groups
> "Materials & Welding" group.
> To unsubscribe from this group and stop receiving emails from it, send an
> email to materials-welding+unsubscribe@googlegroups.com.
> For more options, visit https://groups.google.com/groups/opt_out.
>
>
>
--
*Ramin Kondori*
*Sr. QA/QC Engineer
*
*SINOPEC*
r.kondori@petroyada.com
+98-2123592322
+98-9132150320
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
Subscribe to:
Post Comments (Atom)
[MW:35668] Selection of Filler/Electrode.
Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...
-
Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? ...
-
Definition of buttering from ASME Section IX, QW/QB-492 Definitions: Buttering: the addition of material, by welding, on one or bot...
-
Section I. PRINT READING 3-1. GENERAL a. Drawings . Drawing or sketching is a universal language used to convey all necessary information to...
No comments:
Post a Comment