Please refer 7.4 clause completely whcih is referring to clause 7.3.2.1.
 
Batch Means " When the heat treatment is performed in the enclosed furnace and has to enterrupt (start/stop) for each batch of forgings.
 
Continuos Run Means " When the furnace is having a moving bed..i.e forging on the moving bed enters the furnace at one end & by the time it exits from the other end it has been heat treated to the requirement".
 
Hardness to be done per heat if the the temperature of the furnace is maintained within +/- 14 deg. centigrade both in case of batch and continuos run.
 
Regards,
 
Dokku Ajay Kumar
Mobile: +971-509075925
From: Vino Varghese <vinopvarghese@gmail.com>
To: materials-welding@googlegroups.com
Sent: Monday, January 28, 2013 12:04 PM
Subject: [MW:16620] Query / ASME Sec II Part A / SA 105

Dear All,

Please find the below Query and assist to provide a definition in terms of ASME Reference.

Technical Query:
Reference: ASME Sec II Part A, SA-105 , 7.4 – Hardness Tests
What is the definition of "Batch" and "Continuous Run" as addressed in 7.4 to determine the minimum number of hardness test required for forging? Please provide this definition with a reference in ASME Standard.
 
Anticipating a response ASAP.

Regards,
Vino -Qatar
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 


No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...