We have an issue where the Customer is going around on the a stainless steel (S316L) using a potable to check on the materials and welds

 

He has checked on some areas near the weldment where there is a force of attachment and the magnet is still sticking to the area

The magnet drops off when the magnet is moving away from the weldment

 

I request for a technical understanding to clarify with the customer

 

Appreciate your kind assistance  

 