Re: [MW:16380] Final welding appearance


Contcat your design department.

Attached is the ASME B31.8 -2010 excerpt:

 " Fig. I5 Acceptable Design for Unequal Wall Thickness"


Relevant NOTE: to the figure attached.
(1) No minimum when materials joined have equal specified minimum yield strengths.


ವಂದನೆಗಳೊಂದಿಗೆ / Best regards,

Nandesh Kumar A

Abu Dhabi, UAE

P.S. : Please don't print this e-mail unless you really need to.


--- On Sun, 30/12/12, Samir Mehta <samirmehta.jnd@gmail.com> wrote:

From: Samir Mehta <samirmehta.jnd@gmail.com>
Subject: Re: [MW:16376] Final welding appearance
To: materials-welding@googlegroups.com
Date: Sunday, 30 December, 2012, 5:17 AM

Pls find the attached pic. and advice as the spool is hold by quality control dept, they want me to fill the taper area, and i am not agreed cos its not bevel, pls provide some proof. 

On Sat, Dec 29, 2012 at 7:05 PM, sreekanth <forusree99@rediffmail.com> wrote:

sir,


method -1 is correct as per asme sec ix



Regards,
srikkanth




On Sat, 29 Dec 2012 13:37:52 +0530 wrote

>Dear all,
kindly go through the attached file and advice which one is correct and acceptable method as
per the welding standard also provide reference documents.
regardssamir



--
>
To post to this group, send email to materials-welding@googlegroups.com
>
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
>
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
>
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
>

>
The views expressed/exchnaged in this group are members personel views and meant for
educational purposes only, Users must take their own decisions w.r.t. applicable
code/standard/contract documents.
>

>

>


Catch India as it happens with the Rediff News App. To download it for FREE, click here

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 



--
Samir Mehta
Engineer - Welding & Projects
JPIOS
Abu Dhabi - UAE
+971 55 94 25 327

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...