Re: [MW:16366] Temp. reduction in sub size specimen for Charpy impact test

cuba refer asme B31.3 clause ni..  323.2.2 Lower Temperature Limits, Listed Materials

On Sat, Dec 29, 2012 at 3:17 PM, Farhang <hyperm2m@gmail.com> wrote:

Dear All

I need to know way of calculation temperature reduction when we use sub size specimen.

My problem:

I have tested an A333 Gr.6 (4" pipe-6.3 mm thickness). Labratoary used a sub size specimen (55*5*10). and they tested it in -48c. test temperature of A 333 Gr.6 is -45C and they tested it in 3c cooler temperature Unfortunately absorbed energy was low and my test failed.

But i see a clause in standard(SA-333/SA-333M) which described that:

" 14.1.2) When sub size Charpy impact specimens are used and the width along the notch is less than 80% of the actual wall thickness of the original material "

Is this clause applicable for my case??????

Really i don't know which one is correct?
  • (5/6.3) * 100 = 79% then i should not apply the above mentioned clause and i shall calculate reduction temperature and test my sample in cooler temperature(-45-3=-48).
  • (10/6.3) * 100 = 159% then i should not apply the above mentioned clause and no need to reduction temperature and test my sample in MDMT(-45).

** In the above text i use different color for digits because you can trace them easier.


Many Thanks
Farhang

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 



--
Regards,

Hafizan Bin Harun
Phone : +60129583732
Email: hafizanbh@gmail.com


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...