Re: [MW:16358] Plugging of incorrectly opened drain nozzle opening at 5Cr-1Mo Shell of Heat Exchanger( 2" 300# - Shell thickness : 26 mm.)

Dear Sir,

The best solution is place the nozzle there itself with a flange and box-up it with a blind flange.The nozzle height can be reduced as required, because it is of no use for you. Make a new hole in the correct place and put the required nozzle.

Regards,


On Fri, Dec 28, 2012 at 3:06 PM, Emre Çelebi <mrclbi@gmail.com> wrote:
Dear all,

Please advice that if it is applicable to put and butt weld insert plate for the mentioned incorrectly opened nozzle or should we replace the whole plate?

and, any code/spec. reference?
Regards

Emre Çelebi

QA/QC Supervisor

Açıklama: Açıklama: Açıklama: Açıklama: Açıklama: cid:image001.jpg@01C87261.B13788A0

İzmit Refinery

Investments Department

Resid Upgrading Project (RUP)

Phone   : 0 262 316 1239

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 



--
----------------------
Hareesh K V
+91-9447625012

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...