Thursday, December 27, 2012

Re: [MW:16353] Grinding or filling is allowed on Final pass (on capping) for WPQT ? Urgent plse..

Mr. Sathis kumar,

Codes do not specify about the grinding & filling, on not only final but even in filler passes. It is the discrepancy
of the Inspection authority who witnesses the test. Some allow it while few do not. They feel it is lack of skill on the part of the welder concerned if he is allowed to grind such surface defect.

But, it need not be a fact. Say  if it is a surface pore due to sudden breeze or to other reasons where welder is not at fault, he takes the Inspector into confidence to remove such defects by grinding or other means.  So it is a selective thinking.

More attention is given in initial visual inspection for root defects like. LP, LF, UC,  Ex. Penetration , Oxidation (in TIG process), Cavities, under flush etc., than on surface defects on cap runs.

Sridhar.

From: Sathish Kumar <sathishbemech@gmail.com>
To: materials-welding@googlegroups.com
Sent: Thursday, 27 December 2012 2:37 PM
Subject: [MW:16349] Grinding or filling is allowed on Final pass (on capping) for WPQT ? Urgent plse..

Dear Experts,
Please advice.
whether Grinding or filling is allowed on Final pass (on capping) for Welder performance qualification test (WPQT) for Plate or Pipe. Since qualification is done based on ASME Sec 9, so i need reference only as per ASME Sec 9.
Also already i referred ASME Sec 9 - QW194, which only mentions the Complete joint penetration for visual examination for WPQT. But it is not more specific in case of Grinding or filling and also some other (acceptable limits ? )parameters like Reinforcement, undercut, underfill etc..
I need only Asme Sec 9 reference, because as per the project contract only Asme Sec 9 is applicable for our project in case of WPQT.
please advice guys..
Thanks in advance..
 
Regards
sathish. K
Welding inspector.
Jubail, Saudi arabia.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 


No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...