Dear Kishor

How it ll be above 10mm???????

Fillet sizes has to be calculated with ref to the thinner part joined.........
There its 10mm than hw come it possible to exceed that thk?????


Regards
Ambrish


On Wed, Dec 26, 2012 at 3:26 PM, kishor kaku <kkaku067@gmail.com> wrote:
Dear Ambrish,

Weld metal will be more than 10 mm


Regards


On Tue, Dec 25, 2012 at 12:19 PM, Ambrish Sivakumar <ambrisiva89@gmail.com> wrote:
Dear Avinash

Simply we can qualify with 70 to 80% of weld metal thickness with
refference to thinner metal joined. i.e if u r welding 10mm to 20mm
means weld thick can be around 7-8mm.


Regards
Ambrish
Sr. Engg. - QA

On 12/24/12, Avinash Pandey <avi7589@gmail.com> wrote:
> Dear Expert
>
> Please help me out regarding a query.
>
> 1. If I will be welding 10thk # 20thk plate test coupon of P-No.1 and
> P-No.11A than how much base metal as well as weld metal will be qualify.
>
> 2.Please also give me the interpretation for QW.202.4 (Dissimiler metal
> thickness clauses) in simple english, taht will be very helpful to me
>
> Regards
> Avinash Pandey
>
> Trainee
> Welding Dept.
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to
> materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg at
> http://materials-welding.blogspot.com/
> http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
>
> The views expressed/exchnaged in this group are members personel views and
> meant for educational purposes only, Users must take their own decisions
> w.r.t. applicable code/standard/contract documents.
>
>
>

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm

The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.




--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...